Chinese | English Create new materials, coalesce all things in symbiosis.

Clean Material Bonding

Solution

DP Heat-Curing Series for Cleanroom Panels


DP12 

Mix Ratio100:25
ApplicationCurtain coating
Viscosity (25℃)8000-14000mPa·s
Pot Life4-6min
Open Time19-23min
Pressing Time
5min @60°C to initial cure (Pure Rock Wool)

DP12-17 

Mix Ratio100:25
ApplicationCurtain coating
Viscosity (25℃)8000-14000mPa·s
Pot Life1.5-3.5min
Open Time40-45min
Pressing Time5min @60°C to initial cure (Pure Rock Wool)

DP09D 

Mix Ratio100:25
ApplicationCurtain coating
Viscosity (25℃)8000-14000mPa·s
Pot Life2-4min
Open Time12-14min
Pressing Time5min @60°C to initial cure (Pure Rock Wool)

DP09X 

Mix Ratio100:25
ApplicationCurtain coating
Viscosity (25℃)8000-14000mPa·s
Pot Life5-8.5min
Open Time28-36min
Pressing Time5min @60°C to initial cure (Pure Rock Wool)

DP09X-17 

Mix Ratio100:25
ApplicationCurtain coating
Viscosity (25°C)8000-14000mPa·s
Pot Life7-12min
Open Time40-45min
Pressing Time5min @60°C to initial cure (Pure Rock Wool)


Room-Temperature Curing Series for Cleanroom Panels

SY8401

Mix Ratio100:25
ApplicationCurtain coating / Manual application
Viscosity (25℃)20000-30000mPa·s
Pot Life16-22min
Open Time60-65min
Pressing Time6-8h

SY8410D 

Mix Ratio100:25
ApplicationCurtain coating / Manual application
Viscosity (25℃)10000-20000mPa·s
Pot Life14-20min
Open Time80-100min
Pressing Time8-10h

SY8430 

Mix Ratio100:25
ApplicationCurtain coating / Manual application
Viscosity (25℃)20000-30000mPa·s
Pot Life15-21min
Open Time60-65min
Pressing Time6-8h